E-max or zirconia veneers: which is better?
E-max (lithium disilicate) has the longer record as a veneer and bonds more strongly to the tooth. In a review of 29 studies, 96.81% of lithium disilicate veneers were still in place at about 10 years, with few problems (Klein 2024). Zirconia is stronger and hides a dark tooth better, but its veneer studies only run to about 2 to 3 years so far, and in one 3-year comparison more zirconia veneers came loose and had to be bonded back on. For most healthy front teeth, E-max is the proven choice. Zirconia makes sense for a dark tooth, a heavy bite or very thin designs, with a clinic that follows a careful zirconia bonding protocol.
- Lithium disilicate veneers: 96.81% still in place at about 10 years in a review of 29 studies (Klein 2024).
- Zirconia veneers: no failures at about 2.6 years in the same review, but no long-term data yet.
- Bond strength in lab tests: about 25.4 MPa for lithium disilicate and 12.1 MPa for translucent zirconia (Hajeer 2026).
E-max and zirconia veneers at a glance
| E-max (lithium disilicate) | Zirconia | |
|---|---|---|
| What it is | Glass ceramic | Oxide ceramic, no glass |
| How it is made | Pressed or milled, then fired | Milled from a block, then baked hard |
| Light passing through | More, close to enamel | Less; newer translucent types close part of the gap |
| Strength | About 420 to 500 MPa | About 400 to 1,500 MPa, by type |
| How it grips the tooth | Etched and bonded; a very strong bond | Cannot be etched like glass; needs sandblasting and a special primer |
| Longest veneer studies | 20 years | About 2 to 3 years |
| Still in place | 96.81% at about 10 years (Klein 2024) | No failures at about 2.6 years (Klein 2024) |
| Hides a dark tooth | Moderately | Better |
| On our list | Emax Press, Lisi Press | Origin Beyond Plus, Origin Beyond Multi-Y, Origin Apex, Pearl |
Strength ranges are from Zhang and Lawn (2018); survival from the Klein 2024 review of 29 studies. Each row is explained below. E-max is a brand of lithium disilicate made by Ivoclar; people often use "E-max" for any lithium disilicate.
What is the difference between E-max and zirconia?
Both are ceramics, both are metal-free, and both are made by a dental lab from a scan of your prepared teeth. They behave differently because of what they are made of.
- Lithium disilicate is a glass ceramic: tiny crystals held in glass. Light passes into it much as it passes into enamel. The glass can be etched with acid, which gives the cement a very strong grip.
- Zirconia (zirconium oxide) is a dense crystal ceramic with no glass. It is the strongest tooth-coloured material in use. It was first made for crowns and bridges, and only recently has it been made thin and see-through enough for veneers.
- "Zirconia" is many materials. The more light a zirconia lets through, the weaker it becomes, so translucent zirconias made for front teeth are much less strong than the classic kind used for molars (Zhang and Lawn 2018).
For crowns the two are close, and our page on zirconia and E-max crowns covers them. For veneers the balance is different, because a veneer is thin and depends almost entirely on how well it is glued to the tooth.
Why the bond matters more for veneers
A crown wraps the whole tooth and is held partly by its shape. A veneer is a thin shell on one surface, so it stays on almost only because of the bond. That is where the two materials differ most.
- E-max is etched with hydrofluoric acid and coated with a primer, and the cement locks into the etched glass. This is a well-tested routine.
- Zirconia has no glass to etch. It needs sandblasting with fine alumina and a primer or cement containing a special molecule called MDP. Reviewers describe resin bonding of high-strength ceramics as more complex and more sensitive to technique than plain cementing (Blatz 2018).
- In a review of six lab studies, lithium disilicate veneers bonded with light-cured cement reached about 25.4 MPa of bond strength, and translucent zirconia about 12.1 MPa (Hajeer 2026). Lab numbers are not clinical results, and the studies varied a lot.
In practice this means the zirconia veneer is only as good as the clinic's bonding routine. Ask exactly how they treat the inside of a zirconia veneer before it is bonded.
How long does each last?
| Study | Material | What it found |
|---|---|---|
| Klein 2024, review of 29 studies | Lithium disilicate | 96.81% still in place at about 10 years; technical problems such as chips in 6.1% |
| Aslan 2019, 413 veneers | Pressed lithium disilicate | 98% at 5 years, 95% at 10, 91% at 15, 87% at 20 |
| Klein 2024 | Zirconia | No failures at about 2.6 years; no long-term data |
| Taraszkiewicz-Sulik 2025, 201 veneers | Ultra-thin no-prep zirconia | 99.5% at 2 years, no debonding |
| Nguyen 2025, randomised trial, 52 patients | Zirconia vs lithium disilicate | Both high survival at 1 year, no significant difference |
| Măroiu 2026, 100 veneers and partial covers | A modified zirconia vs lithium disilicate | Neither lost at 3 years; 12% of zirconia and 0% of lithium disilicate came loose and were rebonded |
- Lithium disilicate is one of the most-studied veneer materials, with results out to 20 years.
- Zirconia veneers look good in the early studies, but the longest are 2 to 3 years. Problems that show up at 5 or 10 years, if any, are not known yet.
- The 3-year comparison was small, and the two groups used different cements and different teeth, so its authors call the debonding result exploratory (Măroiu 2026). It is still the clearest early signal: retention is the thing to watch with zirconia.
Which looks more natural?
Natural teeth let some light through, most of all at the biting edge. A veneer that lets light through blends in more easily; one that blocks light can look flat if the shade and the lab's layering are not right.
- In a lab test of 0.5 mm samples, E-max let through about 40% of light and the zirconias tested about 28% to 34% (Harada 2016). At 1.0 mm the order stayed the same.
- Newer multilayer zirconias are more see-through at the edge and stronger near the gum, which closes part of the gap.
- On a healthy, light tooth, either can look natural. The shade, the shape, the surface texture and the lab's finish decide the look far more than the material.
Hudson has watched many shade choices, and he says almost every patient asks for the same thing: natural, with a little see-through quality at the edge. Both materials can give that. Look at the trial smile and the try-in in daylight, next to your own teeth.
Which hides a dark tooth better?
A dark tooth, from an old root canal, a deep stain or a grey band, shows through a very see-through veneer. This is where zirconia's lower translucency helps.
- In a lab test of four veneer materials on dark backgrounds, the colour change was largest for feldspathic porcelain, then E-max, then high-translucency zirconia, then a zirconia-reinforced glass ceramic. The cement shade also made a difference (Sen 2024).
- E-max can still hide moderate darkness with enough thickness. In another lab test, pressed E-max about 0.8 mm thick hid a very dark background within the range people accept as a match (Shadman 2015).
- So for a dark tooth, the choice is between more thickness with E-max, which may mean cutting more tooth, or a less see-through material such as zirconia.
Whitening, or whitening a dead tooth from the inside, can lighten the base first, which may let you keep a thinner veneer. Ask the dentist how dark the tooth is and what they plan for it.
Which is stronger, and does it matter?
Classic zirconia is two to three times as strong as E-max, and even the most translucent zirconias are about as strong as E-max (Zhang and Lawn 2018). But a veneer rarely fails because the material is too weak. It fails at the bond, at a thin edge, or because of grinding.
- Over about 10 years, 6.1% of lithium disilicate veneers had a technical problem such as a chip (Klein 2024). Most chips are small and are polished or repaired.
- Grinding raised the risk of veneer failure 7.7 times in a 20-year study of glass-ceramic veneers (Beier 2012). For a grinder, a night guard matters more than the material.
- Zirconia's strength helps where the veneer is very thin, where the front teeth meet edge to edge, or where a veneer wraps far over the biting edge.
How much of my tooth is removed?
Both can be made thin, so the material does not have to mean more cutting. Ivoclar asks for at least 0.3 mm for a pressed E-max veneer. Zirconia veneers can also be milled thin, and some are bonded with no cutting at all on suitable teeth. This is what our partner clinic's sheet lists for each veneer on our list:
| Veneer | Material | Enamel removed |
|---|---|---|
| Emax Press | Lithium disilicate | 0.3 to 0.5 mm |
| Origin Beyond Plus | Zirconia | 0.3 to 0.5 mm |
| Lisi Press | Lithium disilicate | 0.2 to 0.4 mm |
| Origin Beyond Multi-Y | Zirconia | 0.2 to 0.4 mm |
| Pearl | Zirconia | Ask the clinic |
| Origin Apex | Zirconia | 0.2 to 0.3 mm |
The real amount depends on your teeth and the design more than on the material. A tooth that needs to move back, or a dark tooth that needs hiding, needs more room whatever the veneer is made of.
Which should I choose? Choice by situation
| Your situation | Usual choice | Why |
|---|---|---|
| Healthy, light front teeth, new colour and shape | E-max | The longest record and the strongest bond |
| One or two veneers next to your own teeth | E-max | Its translucency is easier to match to natural enamel |
| A dark or root-filled tooth | Zirconia, or thicker E-max | Zirconia hides darkness with less thickness |
| Front teeth that meet edge to edge | Zirconia, with a bite check | More strength at a thin, loaded edge |
| You grind or clench | Either, plus a night guard | Grinding is the main risk for both |
| No-prep veneers on small or worn teeth | Either; ask which the clinic has done most | Both can be made very thin; early zirconia results are good |
| You want the most proof behind your choice | E-max | Results out to 20 years against about 3 for zirconia |
You can mix them in one smile, for example zirconia on one dark tooth and E-max on the rest. The lab then has to match the two, so check them side by side at the try-in.
The veneers on our list in Vietnam
| Veneer | Material | Made by | Lab warranty | Per tooth |
|---|---|---|---|---|
| Emax Press | Lithium disilicate | Ivoclar, Liechtenstein | 10 years | A$328 |
| Origin Beyond Plus | Zirconia | B&D Dental, USA | 10 years | A$400 |
| Lisi Press | Lithium disilicate | GC, Japan | 10 years | A$428 |
| Origin Beyond Multi-Y | Zirconia | B&D Dental, USA | 12 years | A$571 |
| Pearl | Zirconia | A lab line name; maker not confirmed | 16 years | A$665 |
| Origin Apex | Zirconia | B&D Dental, USA | 15 years | A$971 |
- Emax Press is Ivoclar's pressed lithium disilicate, the material in most of the long veneer studies. Lisi Press is GC's pressed lithium disilicate.
- The three Origin veneers are zirconia blanks made by B&D Dental in the USA. Multi-Y is a multilayer zirconia, more see-through at the edge.
- Pearl is a zirconia veneer sold under a lab's line name. We could not confirm who makes the blank, so ask for the lot certificate if that matters to you.
- The zirconia veneers carry longer lab warranties. A warranty is the lab's promise to redo the veneer, not evidence of how long it lasts; for zirconia veneers the long studies do not exist yet.
A dearer veneer does not look more natural. The shade, the shape and the lab's finish decide the look, and you see them on the trial smile and at the try-in before anything is bonded.
What this means for a veneer trip from Australia
- The material does not change the trip. Veneers take one trip of about 7 to 8 days, with the try-in before bonding.
- If you choose zirconia, ask before you fly how the clinic bonds it, and keep the answer in writing.
- A veneer that comes loose but is not broken can usually be bonded back on. Any dentist at home can do that, so bring your records with the material and the cement used.
- Wear a night guard if you grind, whichever material you choose.
What to ask before you choose
- Which material do you suggest for each of my teeth, and why?
- For zirconia: how do you treat the inside of the veneer before bonding, and which primer or cement do you use?
- How many veneers of this material has the clinic placed, and for how long?
- How much enamel will you remove with each material?
- Is my tooth dark enough that it needs a less see-through material?
- Can I see the material and brand on my plan and my warranty card?
- Will I see the veneers in my mouth, with try-in paste, before they are bonded?
Common beliefs that are not quite right
- "Zirconia is stronger, so it lasts longer." For veneers, the bond decides most failures, and lithium disilicate has the stronger bond and the longer record.
- "Zirconia always looks fake." Classic zirconia is opaque, but translucent and multilayer types can look natural with good shade and shape work.
- "E-max cannot hide a dark tooth." It can hide moderate darkness with enough thickness; zirconia does it with less.
- "A longer warranty means the material is proven." A warranty is a promise from the lab. Zirconia veneers have about 3 years of studies so far.
- "Zirconia veneers need more tooth cut." Both can be very thin; the design decides the cut.
How does The Hudson help?
The Hudson is not a clinic. We are a small team in Hanoi. We audit every clinic we work with and pick the one we trust most for each case. We show you every veneer material on the list with its warranty and price, ask the clinic which one suits each of your teeth and why, and check how they bond it. You choose. Someone from our team comes to every appointment with you, including the shade choice and the try-in.
How we make money
You don't pay us anything. When you go ahead with treatment, the clinic pays us a referral fee for each patient. It doesn't change your price: you pay the clinic's normal price, the same as if you walked in yourself.
Quick answers
Are E-max veneers better than zirconia veneers?
For most healthy front teeth, E-max is the safer choice: it bonds more strongly and has results out to 20 years. Zirconia suits dark teeth and heavy bites, but its veneer studies are only about 3 years long.
Do zirconia veneers look natural?
They can. Translucent and multilayer zirconias let through less light than E-max but much more than classic zirconia. The shade, shape and lab finish decide the look.
Do zirconia veneers fall off more?
Early studies suggest they may come loose more often. In one 3-year comparison, 12% of zirconia and none of the lithium disilicate restorations needed rebonding. The clinic's bonding routine matters.
How long do E-max veneers last?
In a review of 29 studies, 96.81% of lithium disilicate veneers were still in place at about 10 years. One study of 413 pressed veneers found 87% at 20 years.
Is Lisi Press the same as E-max?
Both are pressed lithium disilicate, from different makers: E-max from Ivoclar and Lisi Press from GC in Japan. They behave much alike.
Which costs more in Vietnam?
On our list, Emax Press costs A$328 a tooth and the zirconia veneers A$400 to A$971. Choose by your teeth, not the price.
Not sure which veneer material suits your teeth?
Send us a few photos of your smile. We will ask our partner clinic in Vietnam which material suits each tooth and why, with every option and its price side by side. Free.
Ask about my teethSources
- The Hudson price list, November 2026 (partner clinics in Vietnam). Enamel figures and warranties: our partner clinic's 2026 veneer sheet.
- Klein P et al. Survival and complication rates of feldspathic, leucite-reinforced, lithium disilicate and zirconia ceramic laminate veneers: a systematic review and meta-analysis. J Esthet Restor Dent, 2024.
- Hajeer O et al. Retention of lithium disilicate and translucent zirconia veneers bonded with light-cured resin cements: a systematic review and meta-analysis. Saudi Dent J, 2026.
- Măroiu AC et al. Three-year clinical outcomes of lithium disilicate and lithium-silicate-modified zirconia veneers and partial-coverage restorations: a retrospective comparative study. Dent J, 2026.
- Nguyen VA et al. Clinical performance of zirconia veneers bonded with MDP-containing polymeric adhesives: a one-year randomized controlled trial. Polymers, 2025.
- Taraszkiewicz-Sulik K et al. Two-year clinical performance of ultra-thin no-prep veneers from 5Y-TZP zirconia: a retrospective study. Bioengineering, 2025.
- Aslan YU, Uludamar A, Özkan Y. Clinical performance of pressable glass-ceramic veneers after 5, 10, 15, and 20 years: a retrospective case series study. J Esthet Restor Dent, 2019.
- Zhang Y, Lawn BR. Novel zirconia materials in dentistry. J Dent Res, 2018.
- Blatz MB, Vonderheide M, Conejo J. The effect of resin bonding on long-term success of high-strength ceramics. J Dent Res, 2018.
- Harada K et al. A comparative evaluation of the translucency of zirconias and lithium disilicate for monolithic restorations. J Prosthet Dent, 2016.
- Sen N, Sermet B. Masking ability of monolithic CAD/CAM laminate veneers over different resin cement shades and substrate colors. Int J Prosthodont, 2024.
- Shadman N et al. The minimum thickness of a multilayer porcelain restoration required for masking severe tooth discoloration. Dent Res J, 2015.
- Beier US et al. Clinical performance of porcelain laminate veneers for up to 20 years. Int J Prosthodont, 2012.
- Ivoclar. IPS e.max Press: information from the lab to the dentist (minimum veneer thickness).
- B & D Dental Corp. Origin Beyond Plus zirconia mill blanks: US FDA device record (GUDID).