Dental FAQs

What are Katana zirconia crowns, and how long do they last?

Katana is a range of zirconia made by Kuraray Noritake Dental, a Japanese company. A dental lab mills your crown from a Katana disc after a 3D scan of your teeth. Katana is not one material: the maker sells strong grades for back teeth and bridges (HT and HTML Plus, about 1,125 to 1,150 MPa) and more see-through grades for front teeth (STML at 748 MPa and UTML at 557 MPa), plus YML, which blends the two in one disc. Clinical studies of Katana itself are short and small but good: 20 Katana HT crowns were all still in place after 3 years (Kasem 2022), and 50 Katana STML crowns all lasted 2 years (Hausdörfer 2026). For solid zirconia crowns as a group, 96.8% were still in place after 5 years in a 2026 review of 64 studies (Pjetursson 2026). At our partner clinics in Vietnam a Katana crown costs A$222 a tooth with a 7 years lab warranty, the lowest price on our crown list. Ask which Katana grade the lab uses for each tooth.

  • Katana grades, maker's figures: HTML Plus 1,150 MPa, HT 1,125 MPa, STML 748 MPa, UTML 557 MPa; YML runs from 750 MPa at the edge to 1,100 MPa at the base.
  • Katana HT crowns: 20 of 20 in place at 3 years (Kasem 2022). Katana STML crowns: 50 of 50 in place at 2 years (Hausdörfer 2026).
  • Katana at our partner clinics in Vietnam: A$222 per tooth, 7 years lab warranty.

Katana at a glance

QuestionAnswer
Who makes itKuraray Noritake Dental, Japan
What it isZirconia discs that a lab mills into crowns and bridges
GradesHT, HTML Plus, STML, UTML and YML
Strongest grade, maker's figureHTML Plus, 1,150 MPa
Most see-through grade, maker's figureUTML, 557 MPa, for front teeth
Longest clinical study of Katana crowns3 years: 20 of 20 Katana HT crowns in place (Kasem 2022)
Lab warranty at our partner clinics7 years
Level on our listStandard
Price per tooth in VietnamA$222

A crown is a cap that covers a whole tooth. Zirconia is a strong white ceramic, a kind of what most people call porcelain. MPa (megapascal) is a unit of strength in a bending test: the higher the number, the more force the material takes before it breaks. Prices from our partner clinics' list, updated Nov 2026.

Who makes Katana?

Kuraray Noritake Dental, a Japanese dental materials company. Katana is its zirconia brand. Kuraray sells Katana as discs and blocks to dental labs; the lab designs your crown on a computer from a scan of your teeth, mills it from the disc, fires it hard in an oven, then stains, glazes or polishes it.

  • So a "Katana crown" means a crown milled from Katana zirconia. The lab's design, shade and finish are as much a part of the result as the disc.
  • Katana is used widely in dental research: a PubMed search in November 2026 found about 215 records that mention Katana zirconia, most of them lab tests.
  • Kuraray Noritake also makes other materials under the Katana name, such as Katana Avencia, a resin-based block. Those are not zirconia and are not on our crown list.

The Katana grades, and where each suits

GradeStrengthLight throughLayersMaker's main uses
HTML Plus1,150 MPa45%Multilayer shadesCrowns and bridges, including long bridges
HT1,125 MPa45%One colour (white disc)Frames under layered porcelain, full-contour crowns and bridges
YML750 MPa at the edge to 1,100 MPa at the base49% at the edge to 45% at the baseStrength and colour gradientFront and back crowns, 3-unit and long bridges
STML748 MPa49%Multilayer shadesCrowns and bridges up to 3 units
UTML557 MPa51%Multilayer shadesFront crowns and front bridges up to 3 units
  • The trade-off is the same in every zirconia range: the more light a grade lets through, the more it looks like enamel, and the less strong it is.
  • "HT" stands for high translucency, but in Katana's range HT and HTML Plus are the strong, least see-through grades. STML is "super" and UTML "ultra" translucent.
  • The light figures are the maker's own and close together (45% to 51%). Lab tests disagree on how see-through the clearest grades are. In one 2026 test, all four multilayer Katana grades let through far less light than two lithium disilicate (E-max type) ceramics (Dejak 2026); in another, Katana UTML was as see-through as pressed E-max (Flask 2022). Thickness and test method change the result.
  • YML builds the gradient into one disc. Where in the disc the lab places the crown changes its strength: in one test, premolar crowns cut from the lower, stronger part broke at higher loads, and crowns from the upper part were more see-through (Imaemporn 2025).
  • Lab studies that measured the exact chemistry of Katana grades do not all agree on how much yttria (the stabiliser) each contains (Shishido 2023; Alghazzawi 2023). The maker's grade name and strength are the reliable guide.

For what 3Y, 4Y and 5Y mean, and how strength trades against see-through across all brands, read our page on the types of zirconia, linked under Read next.

Which Katana is on our price list?

Our list names the brand, Katana, not the grade. Because one brand covers grades from 557 to 1,150 MPa, ask the clinic which Katana disc the lab uses for each of your teeth. For back teeth the usual answer is a strong grade such as HT, HTML Plus or the base of YML. For a single front tooth next to your own teeth, a lab may use STML or UTML.

  • Ask for the grade per tooth in writing, on your treatment plan.
  • Ask for the lab card or the label with the product name after the crowns are made.
  • If you grind your teeth, ask for a strong grade and a night guard.

What clinical studies of Katana show

These are the studies in patients we found that name a Katana grade for the crowns. All are short and small, so they show that Katana crowns do well in the first years, not how they do at 10.

StudyWhat was testedWhat it foundLimits
Kasem 2022, Egypt and Switzerland20 Katana HT crowns on root-filled upper premolars, with a gentle (vertical) preparationAll 20 still in place at 3 years; no fractures or other mechanical problemsSmall; one tooth type
Hausdörfer 2026, Göttingen, Germany50 Katana STML crowns against 50 crowns of a milled lithium disilicateAll 50 Katana crowns survived 2 years; 82% of the glass ceramic crowns survived, with 10 brokenAt least 2 years only; one study
Di Fiore 2021, Padova, ItalyKatana ML (multilayer) crowns and bridges on 51 back-tooth implants96% of implants and crowns in place at 3 years; the two losses were implants, not crowns; 2 loose screwsImplant study; the crowns were not the main question
Yang 2018, Yonsei University, Korea15 Katana crowns on implants replacing molarsKatana wore the opposite teeth more than another zirconia in the first 6 months6 months; wear only
Sagirkaya 2012 and Ozer 2014Katana among several brands used as the core under layered porcelainGood survival overall, reported for all brands togetherOlder layered crowns; Katana not reported alone
  • No Katana crown in these studies broke. That fits the lab data for the strong grades.
  • We found no study of Katana crowns followed for 5 years or longer. That means less is known, not that Katana does worse; for most zirconia brands no long brand study exists.
  • For solid zirconia crowns of any brand, the long record is good: 96.8% were still in place after 5 years in a 2026 review of 64 studies, close to metal-ceramic crowns at 97.1% (Pjetursson 2026).

What lab tests by other groups show

  • Colour over a metal base: in a test of crowns on titanium and zirconia connectors, Katana HT showed the least colour change of four zirconia brands across the different connectors (Patel 2025). Useful for a crown on an implant.
  • Over a metal base: most of the ceramics tested, Katana included, turned noticeably grey over metal, and lithium disilicate most of all (Dejak 2026). A dark base needs a planned answer, such as an opaque layer, whatever the brand.
  • Thin edges: in a lab test on premolars, Katana crowns with a thin 0.5 mm edge held average loads of about 1,256 to 1,348 N after ageing, against about 471 to 483 N for a zirconia-reinforced glass ceramic (Kasem 2020).
  • Front-tooth grade on root-filled premolars: UTML endocrowns (a crown with a stem into the root canal space) withstood higher repeated loads than lithium disilicate ones, but when they broke they usually could not be repaired (Demachkia 2023).
  • Chipping at thin edges: in a test of edge toughness, Katana UTML resisted chipping less (304 N/mm) than pressed E-max (354), Lava Esthetic (394) or the strong Lava Plus (717) (Flask 2022). The more see-through the zirconia, the more care thin edges need.
  • Surface finish matters: grinding and sandblasting change the surface of every Katana grade (Shishido 2023). A crown adjusted in the mouth should be polished smooth again.

Does a Katana crown wear the opposite teeth?

A little more than your own enamel does, and less than older porcelain-on-metal crowns. The polish is what matters most.

StudyWhat it found
Mao 2024, review of 7 studies, 261 crowns, up to 2 yearsZirconia caused about 40 microns more wear on the opposite tooth than enamel against enamel; metal-ceramic about 82 microns more; lithium disilicate about 5 microns more
Rosa 2026, review of 9 studies, 6 to 24 monthsZirconia and lithium disilicate crowns both wore opposite enamel more than enamel against enamel
Yang 2018, Katana on implant molarsKatana wore the opposite teeth more than another zirconia, and its surface changed within 6 months in the mouth

40 microns is 0.04 mm over up to two years. A 2024 network review was summarised as finding that polished zirconia crowns may cause less wear on opposite enamel than metal-ceramic ones (Alqutaibi 2025), so ask for the crowns to be polished smooth. If you grind, a night guard protects both.

How long do Katana crowns last?

  • Katana itself: all crowns still in place at 2 and 3 years in the two studies that followed Katana crowns on natural teeth (Kasem 2022; Hausdörfer 2026).
  • Solid zirconia crowns of any brand: 96.8% in place at 5 years (Pjetursson 2026).
  • What ends a zirconia crown is often not the zirconia: in a 5-year trial of 50 solid zirconia crowns on back teeth, none broke, the one crown lost was to a cracked root, and two came loose (Solá-Ruiz 2021).
  • The lab warranty at our partner clinics is 7 years. That is the lab's promise to remake a crown that fails, not a measure of how long the crown lasts.

Long life depends on the same things for every crown: a good fit, cleaning at the gum line, regular check-ups and a night guard if you grind.

Katana price and warranty in Vietnam

BrandPer tooth16 teeth20 teethLab warranty
Standard
KatanaJapanA$222A$3,560A$4,4407 years
CeramillAustriaA$286A$4,580A$5,72010 years
DD BioGermanyA$333A$5,330A$6,66010 years
Plus
Origin Beyond PlusUSAA$357A$5,720A$7,14010 years
Lava PlusUSAA$444A$7,110A$8,88015 years
Lava EstheticUSAA$554A$8,870A$11,08015 years
Premium
Orodent BleachItalyA$666A$10,050A$12,56019 years
Origin ApexUSAA$971A$15,540A$19,42015 years

Updated Nov 2026

Free flight
& hotel
Claim now
T&Cs apply
How manyPriceHow it is worked out
1 crownA$222Price list, per tooth
4 crownsA$888The per-tooth price times 4
8 crownsA$1,776The per-tooth price times 8
Difference from DD Bio, per toothA$111DD Bio A$333 minus Katana A$222, both from the same list
  • Katana is the lowest-priced crown on our list, with a 7 years lab warranty. DD Bio and Ceramill, in the same level, carry 10 years.
  • A lower price does not mean a weaker or less natural crown. The shade, the shape and the lab's finish decide the look; the grade and the design decide the strength.
  • Root canal treatment, a post or a new filling under the crown are priced separately if a tooth needs them.

Is Katana a good choice for my teeth?

General guidance only. Your dentist decides after seeing your teeth and bite.

Your situationUsual choiceWhy
Back teethKatana in a strong gradeStrong, and the bite is heaviest at the back
A crown on an implantKatana HT or another strong gradeShowed little colour change over metal connectors in one lab test (Patel 2025)
One front tooth next to your own teethAsk about STML or UTML, or Lava EstheticMore light through, to match the tooth beside it
A dark tooth or metal post underneathA less see-through gradeHides the dark base better
You grind your teethA strong grade and a night guardGrinding loads every crown
You want a longer lab warrantyDD Bio or Ceramill, 10 yearsSame level, longer lab warranty

What this means for a crown trip from Australia

  • Katana does not change the number of days. Crowns need one trip of up to 7 days.
  • Ask for the Katana grade per tooth in writing before you fly, and keep the lab card when you leave.
  • If a dentist at home ever adjusts the crown, tell them it is Katana zirconia and which grade, so they polish it with zirconia polishers.
  • Zirconia shows clearly on X-rays, more than any other crown material in one test (Nejat 2025), so your dentist at home can check the edges of the crown on a normal check-up X-ray.

What to ask before you choose

  • Which Katana grade will the lab use for each of my teeth, and why?
  • Will the crowns be solid zirconia, or zirconia with porcelain layered on top?
  • Can I see the shade in daylight next to my own teeth before the crowns are made?
  • Will the crowns be polished, glazed or both?
  • What does the 7 years lab warranty cover, and what must I do to keep it?
  • Can I have the lab card or label with the product name?

Common beliefs that are not quite right

  • "Katana is one material." It is a range of five grades, from 557 to 1,150 MPa.
  • "HT means the most see-through." In Katana's range, HT and HTML Plus are the strong, least see-through grades.
  • "The lowest-priced crown is the weakest." Katana's strong grades are rated at 1,125 to 1,150 MPa by the maker. Price and strength do not track each other.
  • "A short warranty means a short life." The warranty is the lab's promise. Solid zirconia crowns of any brand were 96.8% in place at 5 years (Pjetursson 2026).
  • "Zirconia destroys the teeth it bites against." Zirconia wore opposite teeth less than porcelain-on-metal crowns in a review of patient studies (Mao 2024).
  • "Katana crowns have been studied for decades." The Katana crown studies in patients run to 3 years. The longer record belongs to zirconia crowns as a group.

How does The Hudson help?

The Hudson is not a clinic. We are a small team in Hanoi. We audit every clinic we work with and pick the one we trust most for each case. We show you every crown on the list with its warranty and price, ask the clinic which product and grade the lab uses for each of your teeth and why, and make sure the answer is written on your plan. You choose. Someone from our team comes to every appointment with you, including the shade choice and the fitting.

How we make money

You don't pay us anything. When you go ahead with treatment, the clinic pays us a referral fee for each patient. It doesn't change your price: you pay the clinic's normal price, the same as if you walked in yourself.

Quick answers

What is Katana zirconia?

A range of zirconia discs from Kuraray Noritake Dental in Japan. A lab mills your crown from the disc after a scan of your teeth.

Is Katana zirconia strong?

The strong grades, HT and HTML Plus, are about 1,125 to 1,150 MPa on the maker's figures. The see-through UTML grade is 557 MPa and is meant for front teeth.

What is the difference between Katana STML and UTML?

STML is the middle grade, 748 MPa, for crowns and bridges up to 3 units. UTML is the most see-through, 557 MPa, for front teeth only.

How long do Katana crowns last?

In the two studies of Katana crowns on natural teeth, all crowns were still in place at 2 and 3 years. Solid zirconia crowns as a group were 96.8% in place at 5 years.

How much is a Katana crown in Vietnam?

A$222 per tooth at our partner clinics, with a 7 years lab warranty.

Want to know which Katana grade you would get?

Send us a photo of your teeth or your current quote. We ask the dentist at a partner clinic in Vietnam which crown and grade suits each tooth, and why. Free.

Ask us

Sources